What is the compression of beryllium copper shrapnel? How much is the shrapnel compressed to ensure that it is pressed 100,000 times without deformation? As we all know, the shielding and conductivity of beryllium copper shrapnel will only occur when it is in contact with metal products, so what is the compression amount of beryllium copper shrapnel to make the shrapnel product achieve the best shielding and conductivity performance? Or in other words, how high do we need to compress the beryllium copper shrapnel to extend the service life of the beryllium copper shrapnel, and really achieve 100,000 or even a million times of compression without deformation?
What is the compression amount of beryllium copper shrapnel? The compression of beryllium copper reed is an important parameter for customers to choose shrapnel. How to choose the compression amount, the main considerations are as follows:
1. Product resilience: The compression of beryllium copper shrapnel is too large, which affects the resilience of the shrapnel, resulting in product failure and inability to shield.
2. Compression force requirements: consider how much compression force the beryllium copper shrapnel will receive during the application process.
What is the compression amount of beryllium copper shrapnel? Compression = maximum gap of beryllium copper shrapnel - minimum gap, or compression amount = free height of beryllium copper shrapnel - working height
Recommended compression amount: According to the customer's experience and test basis: it is recommended that the customer use beryllium copper shrapnel The optimal compression amount: 30% (that is, compressed to 70% of the product height)
Reasonable use of compression range: 30%-50%
What Is The Amount Of Compression Of Beryllium Copper Shrapnel